By the Magna technical team · April 2026 · 1 min read
Platinum group metal refining runs hotter than almost any other melt, and the glassy, siliceous slags involved attack most refractories quickly. Lime stabilised zirconia holds up where others fail, with a service temperature to 2200°C.
Its resistance to those slags, combined with a dense body, is what keeps the metal clean and the crucible in service through repeated high temperature pours.
Related articles
All insights
Applications
August 28, 2026
Melting platinum group metals in lime stabilised zirconia
Why platinum refiners choose lime stabilised zirconia, and how it resists glassy slags to 2200°C.
Material selection
August 28, 2026
How to choose the right crucible material for your alloy
Alumina, chrome alumina, zirconia or magnesia: how alloy, temperature and process decide the right crucible.
Material selection
August 28, 2026
What causes inclusions in the melt, and how to reduce them
Where casting inclusions come from, and how a dense, non-wetting crucible keeps the metal clean.
Specify the right crucible for your application
Send the alloy, volume and process you're working with, and our technical team will specify the right crucible.
- Reply from a technical specialist within one working day
- Drawings and specifications welcome
- No obligation